Electrical conductivity σel
1.80E+7 - 2.80E+7 S/m at 20 °C
Density ρ
2.79 - 2.8 g/cm³ at 20 °C
Elastic modulus E
65 - 73.5 GPa at 20 °C
Tensile strength Rm
32 - 436 MPa at 20 °C
Melting point Tm
650 °C
Specific heat capacity cp
921 J/(kg·K) at 20 °C
Thermal conductivity λ
130 - 200 W/(m·K) at 20 °C
Element
Weight %
Comment
3.5 - 4.5 %
0.7 %
0.4 - 1 %
0.4 - 1 %
0.25 %