Koeffizient der thermischen Ausdehnung: 1.03E-5 - 1.05E-5 1/K

Quick Comparison

Kohlenstoffarmer Stahl

EN 10025-3 Grade S420N normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Kohlenstoffarmer Stahl

EN 10025-3 Grade S420NL normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Molybdenum Steel

EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Nickel Molybdenum Steel

EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-3 Grade P460NL1 normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Unclassified Low Alloy Steel

EN 10028-3 Grade P460NL2 normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Nickel molybdenum Steel

EN 10028-2 Grade 15NiCuMoNb5-6-4 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Unclassified Low Alloy Steel

EN 10028-3 Grade P460NH normalized or normalized formed (+N)

Geliefert von:

2 Matmatch-Lieferanten

Nickel Steel

EN 10028-4 Grade 11MnNi5-3 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 13MnNi6-3 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Nickel Steel

EN 10028-4 Grade 15NiMn6 normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Chromium Steel

ISO 683-3 Grade 16MnCr5 normalized or normalized formed (+N)

Geliefert von:

1 Matmatch-Lieferant

Nickel Molybdenum Steel

ASTM A387 Grade 11 Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Martensitischer Edelstahl

ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)

Geliefert von:

1 Matmatch-Lieferant

Seite 1 von 121