General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.41 g/cm³ Show Supplier Material materials with Density of 1.41 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 0.85 % Show Supplier Material materials with Moisture absorption of 0.85 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 1.9 % Show Supplier Material materials with Water absorption of 1.9 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 9.8 GPa Show Supplier Material materials with Elastic modulus of 9.8 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
11.5 GPa Show Supplier Material materials with Elastic modulus of 11.5 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 4.9 % Show Supplier Material materials with Elongation of 4.9 % | dry | ISO 527-2/1A | 5mm/min | |
6.9 % Show Supplier Material materials with Elongation of 6.9 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Flexural modulus | 10.1 GPa Show Supplier Material materials with Flexural modulus of 10.1 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 280 MPa Show Supplier Material materials with Flexural strength of 280 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | -30 °C | 20 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 20 kJ/m² | dry | ISO 179/1eA | |
23 °C | 18 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 18 kJ/m² | dry | ISO 179/1eA | ||
Impact strength, Charpy unnotched | -30 °C | 125 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 125 kJ/m² | dry | ISO 179/1eU | |
23 °C | 115 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 115 kJ/m² | dry | ISO 179/1eU | ||
Tensile strength | 150 MPa Show Supplier Material materials with Tensile strength of 150 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
185 MPa Show Supplier Material materials with Tensile strength of 185 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.8e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.8e-05 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | ||
0.0001 1/K Show Supplier Material materials with Coefficient of thermal expansion of 0.0001 1/K | ISO 11359-1/-2 | ||||
Heat deflection temperature | 205 °C Show Supplier Material materials with Heat deflection temperature of 205 °C | ISO 75/2Af | 1.80 MPa | ||
Melting point | 217 °C Show Supplier Material materials with Melting point of 217 °C | ISO 11357-1/-3 | 10°C/min | ||
Flammability | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 0.3 % Show Supplier Material materials with Shrinkage of 0.3 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Hydrolysis Resistance, Heat Stabilized | |
Fillers | 40% Glass Fiber | |