Dichte: 1.12 - 1.13 g/cm³

Quick Comparison

Polyamide 6 (PA6)

Akulon® F223-D

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K222-D

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® F-X9190

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

Zytel® 7335F NC010

Polyamide 6 (PA6)

Novamid® 1010C2

Geliefert von:

DSM Engineering Materials

Polyamide 4T (PA4T)

Akulon® F232-D

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

Novamid® 1013C5

Geliefert von:

DSM Engineering Materials

Polyamide 6T (PA6T)

Zytel® HTNFE8200 NC010

Thermoplastischer Co-Polyester (TCP)

Hytrel® HTR8223 BK320

Polyamide 6 (PA6)

Novamid® 1013C

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® F136-DH

Geliefert von:

DSM Engineering Materials

Polyphenylether (PPE)

NORYL™ Resin LTA6020 - Europe

Geliefert von:

Sabic

Polyphenylether (PPE)

NORYL™ Resin LTA6020 - Asia

Geliefert von:

Sabic

Polyphenylether (PPE)

NORYL™ Resin LTA6020 - Americas

Geliefert von:

Sabic

Polyamide 6 (PA6)

Zytel® 7301 NC010
Seite 1 von 13