General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.12 g/cm³ Show Supplier Material materials with Density of 1.12 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 2.7 % Show Supplier Material materials with Moisture absorption of 2.7 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 9.2 % Show Supplier Material materials with Water absorption of 9.2 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 1.1 GPa Show Supplier Material materials with Elastic modulus of 1.1 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
2.8 GPa Show Supplier Material materials with Elastic modulus of 2.8 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 90 % Show Supplier Material materials with Elongation of 90 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
100 % Show Supplier Material materials with Elongation of 100 % | 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | ||
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-2/1A | 50mm/min | |
20 % Show Supplier Material materials with Elongation at yield of 20 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Flexural modulus | 2.5 GPa Show Supplier Material materials with Flexural modulus of 2.5 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 95 MPa Show Supplier Material materials with Flexural strength of 95 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | 23 °C | 9 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 9 kJ/m² | dry | ISO 179/1eA | |
Yield strength | 45 MPa Show Supplier Material materials with Yield strength of 45 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
75 MPa Show Supplier Material materials with Yield strength of 75 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermal
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 650 °C Show Supplier Material materials with Glow Wire Flammability Index of 650 °C | 2 mm | IEC 60695-2-12 | ||||
Heat deflection temperature | 60 °C Show Supplier Material materials with Heat deflection temperature of 60 °C | ISO 75/2Af | 1.80 MPa | ||||
165 °C Show Supplier Material materials with Heat deflection temperature of 165 °C | ISO 75/2Bf | 0.45 MPa | |||||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat softening temperature | 185 °C Show Supplier Material materials with Vicat softening temperature of 185 °C | ISO 306 | 50°C/h 50N | ||||
Flammability | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): <30 ,method: ISO 3795 and thickness tested (mm): 3 |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Comparative tracking index | 600 V Show Supplier Material materials with Comparative tracking index of 600 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Shrinkage | 1.2 % Show Supplier Material materials with Shrinkage of 1.2 % | 280/70/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
1.3 % Show Supplier Material materials with Shrinkage of 1.3 % | 280/70/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding,Profile Extrusion |