Kohlenstoffarmer Stahl
EN 10025-2 Grade S235JR as-rolled condition (+AR)Geliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Kohlenstoffarmer Stahl
EN 10025-2 Grade S185 normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Austenitischer rostfreier Stahl
Esshete 1250Geliefert von:
Alleima (formerly Sandvik Materials Technology)Duplex rostfreier Stahl
Sandvik SAF 2205™ Solution AnnealedGeliefert von:
Alleima (formerly Sandvik Materials Technology)Duplex rostfreier Stahl
Sandvik SAF 2205™ Cold WorkedGeliefert von:
Alleima (formerly Sandvik Materials Technology)Kohlenstoffarmer Stahl
DIN 1629 Grade St 37.0 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 1626 Grade USt 37.0 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 1628 Grade St 37.4 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10025 Grade S235J2G3 normalized or normalized formed (+N)Ferritischer Edelstahl
DIN 17440 Grade X3CrTi17 soft annealed (+A)Ferritischer Edelstahl
DIN 17440 Grade X6CrAl13 soft annealed (+A)Kohlenstoffarmer Stahl
DIN 17174 Grade TTSt 35 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17175 Grade St 35.8 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 1630 Grade St 37.4 hot worked, normalizedKohlenstoffarmer Stahl
DIN 5512-1 Grade S235J2G3 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 5512-1 Grade S235JRG2 normalized or normalized formed (+N)