Härte, Vickers: 265 - 325 [-]

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper Nickel Silver Grade

UNS C77000 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper Nickel Grade

UNS C70250 boway

Geliefert von:

Ningbo Boway Alloy Material

Phosphorbronze

UNS C52100 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Phosphorbronze

UNS C52400 boway

Geliefert von:

Ningbo Boway Alloy Material

Phosphorbronze

UNS C51000 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Wrought Copper Nickel Grade

UNS C70250 boway

Geliefert von:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TF00

Alpha-Beta-Legierung

AMS 4907 Grade R56407

Geliefert von:

1 Matmatch-Lieferant

Alpha-Beta-Legierung

AMS 4907 Grade R56407

Geliefert von:

1 Matmatch-Lieferant

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM00 (C72900)

Geliefert von:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM02 (C72900)

Geliefert von:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM04 (C72900)

Geliefert von:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM06 (C72900)

Geliefert von:

Materion Brush GmbH

Wrought Copper Nickel Grade

BrushForm® 158 Strip TM08 (C72900)

Geliefert von:

Materion Brush GmbH