Zytel® 80G33HS1L BK104

Alternative and trade names
PA66-I-GF33
Want to keep this datasheet? Save it now in your required format

Description

Common features of Zytel® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness and toughness, good high temperature performance, good electrical and flammability properties, good abrasion and chemical resistance. In addition, Zytel® nylon resins are available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses. Zytel® nylon resin, including most flame retardant grades, offer the ability to be coloured. The good melt stability of Zytel® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.Zytel® nylon resin typically is used in demanding applications in the automotive, furniture, domestic appliances, sporting goods and construction industry.Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.33 g/cm³

Show Material materials with Density of 1.33 g/cm³

ISO 1183

Water absorption

23.0 °C

0.91 %

Show Material materials with Water absorption of 0.91 %

Sim. to ISO 62 | Immersion 24h

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

8.8 GPa

Show Material materials with Elastic modulus of 8.8 GPa

ISO 527-1/-2

Elongation

23.0 °C

3.6 %

Show Material materials with Elongation of 3.6 %

ISO 527-1/-2

Flexural modulus

23.0 °C

7.6 GPa

Show Material materials with Flexural modulus of 7.6 GPa

ISO 178

Flexural strength

23.0 °C

214 MPa

Show Material materials with Flexural strength of 214 MPa

ISO 178

Hardness, Ball Indentation

23.0 °C

220 MPa

Show Material materials with Hardness, Ball Indentation of 220 MPa

ISO 2039-1

Impact strength, Charpy notched

-40.0 °C

18 kJ/m²

Show Material materials with Impact strength, Charpy notched of 18 kJ/m²

ISO 179/1eA

-6.0 °C

18 kJ/m²

Show Material materials with Impact strength, Charpy notched of 18 kJ/m²

ISO 179/1eA

23.0 °C

20 kJ/m²

Show Material materials with Impact strength, Charpy notched of 20 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

-40.0 °C

109 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 109 kJ/m²

ISO 179/1eU

23.0 °C

97 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 97 kJ/m²

ISO 179/1eU

Unlock all property charts

Impact strength, Izod notched

-30.0 °C

87 kJ/m²

Show Material materials with Impact strength, Izod notched of 87 kJ/m²

ISO 180/1U

Impact strength, Izod unnotched

-40.0 °C

15 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 15 kJ/m²

ISO 180/1A

-30.0 °C

17 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 17 kJ/m²

ISO 180/1A

23.0 °C

21 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 21 kJ/m²

ISO 180/1A

Unlock all property charts

Poisson's ratio

23.0 °C

0.34 [-]

Show Material materials with Poisson's ratio of 0.34 [-]

Tensile strength

23.0 °C

148 MPa

Show Material materials with Tensile strength of 148 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

9E-6 1/K

Show Material materials with Coefficient of thermal expansion of 9E-6 1/K

ISO 11359-1/-2 | 23 - 55°C

Coefficient of thermal expansion, transverse

23.0 °C

1.2E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1.2E-4 1/K

ISO 11359-1/-2 | 55 - 160°C

Heat deflection temperature, 0.45 MPa

261 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 261 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

245 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 245 °C

ISO 75-1/-2

Melting point

262 °C

Show Material materials with Melting point of 262 °C

ISO 11357-1/-3 | 18°F/min

Relative temperature index, electrical

130 °C

Show Material materials with Relative temperature index, electrical of 130 °C

UL 746B | 120mil

Relative temperature index, mechanical impact

105 °C

Show Material materials with Relative temperature index, mechanical impact of 105 °C

UL 746B | 120mil

Relative temperature index, mechanical strength

105 °C

Show Material materials with Relative temperature index, mechanical strength of 105 °C

UL 746B | 120mil

Flammability

Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 0.75 mm, UL recognition: yes -, Glow Wire Flammability Index, 40mil: 650 °C, Glow Wire Flammability Index, 80mil: 700 °C, Glow Wire Flammability Index, 120mil: 900 °C, Glow Wire Ignition Temperature, 40mil: 700 °C, Glow Wire Ignition Temperature, 80mil: 700 °C, Glow Wire Ignition Temperature, 120mil: 750 °C, FMVSS Class: SE -, Burning rate, Thickness 1 mm: 23 mm/min

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.3 %

Show Material materials with Shrinkage of 0.3 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

0.7 %

Show Material materials with Shrinkage, transverse of 0.7 %

ISO 294-4, 2577

Technological properties

Property
Fillers

33% Glass Fiber

Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 295°C, Min. melt temperature: 285°C, Max. melt temperature: 305°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 80°C, Min. mold temperature: 50°C, Max. mold temperature: 100°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm, Ejection temperature: 210°C