Kohlenstoffarmer Stahl
EN 10028-2 Grade P295GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10028-2 Grade P355GH normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Geliefert von:
1 Matmatch-Lieferant
Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Chromium Molybdenum Steel
EN 10216-2 Grade 12CrMo9-10 quenched and tempered (+QT)Kohlenstoffarmer Stahl
EN 10216-2 Grade 19Mn5 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
DIN 17175 Grade St 35.8 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10216-2 Grade St 45.8 normalized or normalized formed (+N)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 soft annealed (+A)Kohlenstoffarmer Stahl
EN 10217-2 Grade St 37.8 normalized or normalized formed (+N)Kohlenstoffarmer Stahl
EN 10217-2 Grade St 42.8 normalized or normalized formed (+N)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT2)Chromium Molybdenum Steel
DIN 17176 Grade 12CrMo19-5 quenched and tempered (+QT1)Kohlenstoffarmer Stahl
DIN 17155 Grade 17Mn4 normalized or normalized formed (+N)