Zugfestigkeit: 0.38 MPa

Quick Comparison

Thermoplastischer Styrol-block-Copolymer (TPS)

TPE-S PHOENIX 05051

Geliefert von:

Phon Tech Industrial Company

Austenitischer rostfreier Stahl

ASTM A487 Grade 8 Class A, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 2 Class C, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 2 Class A, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 4 Class A, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 14 Class A, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 10 Class A, Heat-Treated

Nickel Chromium Molybdenum Steel

ASTM A487 Grade 2 Class B, Heat-Treated
Seite 1 von 2