ASTM A487 Grade 10 Class A, Heat-Treated

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A50

20.0 °C

0 - 18 %

Show Material materials with Elongation A50 of 0 - 18 %

Reduction of area

20.0 °C

0 - 35 %

Show Material materials with Reduction of area of 0 - 35 %

Tensile strength

20.0 °C

0 - 690 MPa

Show Material materials with Tensile strength of 0 - 690 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

0 - 485 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 485 MPa

Chemical properties

PropertyValue

Carbon

0 - 0.3 %

Show Material materials with Carbon of 0 - 0.3 %

Copper

0 - 0.5 %

Show Material materials with Copper of 0 - 0.5 %

Manganese

0.6 - 1 %

Show Material materials with Manganese of 0.6 - 1 %

Molybdenum

0.2 - 0.4 %

Show Material materials with Molybdenum of 0.2 - 0.4 %

Phosphorus

0 - 0.04 %

Show Material materials with Phosphorus of 0 - 0.04 %

Silicon

0 - 0.8 %

Show Material materials with Silicon of 0 - 0.8 %

Sulfur

0 - 0.035 %

Show Material materials with Sulfur of 0 - 0.035 %

Tungsten

0 - 0.1 %

Show Material materials with Tungsten of 0 - 0.1 %

Vanadium

0 - 0.03 %

Show Material materials with Vanadium of 0 - 0.03 %