Kohlenstoffarmer Stahl
EN 10025-2 Grade S235JR as-rolled condition (+AR)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 quenched and tempered (+QT)Geliefert von:
1 Matmatch-Lieferant
Unclassified Low Alloy Steel
EN 10225 Grade S420G1 thermomechanically rolledGeliefert von:
1 Matmatch-Lieferant
Austenitischer rostfreier Stahl
EN 10088-1 Grade X1NiCrMoCu25-20-5 solution annealed (+AT)Austenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-3 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-5 solution heat-treated and quenchedAustenitischer rostfreier Stahl
DIN 17440 Grade X2CrNiMoN17-13-3 quenched (+Q)Austenitischer rostfreier Stahl
EN 10028-7 Grade X2CrNiMo17-12-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10272 Grade X1NiCrMoCu25-20-5 solution annealed (+AT)Near-Alpha-Legierung
DIN 17850 Grade Ti3Pd AnnealedAustenitischer rostfreier Stahl
EN 10088-1 Grade X2CrNiMo18-14-3 solution annealed (+AT)Nickel Chromium Iron Alloy
DIN 17744 Grade NiCr21Mo soft annealed (+A)Austenitischer rostfreier Stahl
DIN 1654-5 Grade X2CrNiMoN17-13-3 quenched (+Q)Nickel Chromium Iron Alloy
DIN 17742 Grade NiCr23Fe solution annealed (+AT)Nickel Chromium Molybdenum Alloy
DIN 17744 Grade NiMo16Cr16Ti solution heat-treated and quenchedNickel Chromium Alloy
DIN 17744 Grade NiCr22Mo7Cu solution annealed (+AT)