Quick Comparison

Acero bajo en carbono

EN 10028-2 Grade P355GH normalized or normalized formed (+N)

Suministrada por:

2 proveedores de Matmatch

Acero bajo en carbono

EN 10025-2 Grade S355JR normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Nickel Molybdenum Steel

EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

EN 10083-3 Grade 20MnB5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

ASTM A36

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

ASTM A709 Grade 345 Type 1

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

ASTM A612 As-Rolled or Normalized and/or Stress Relieved

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

ASTM A709 Grade 345 Type 3

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

ASTM A709 Grade 345 Type 2

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

ASTM A573 Grade 400

Suministrada por:

1 proveedor Matmatch

Acero bajo en carbono

ASTM A709 Grade 250

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Stainless Steel

ASTM A537 Class 1 Normalized

Suministrada por:

2 proveedores de Matmatch

Unclassified Carbon Steel

ASTM A572 Grade 450

Suministrada por:

1 proveedor Matmatch

Nickel Chromium Molybdenum Alloy

VDM® Alloy 602 CA

Suministrada por:

VDM Metals

Unclassified Carbon Steel

ASTM A573 Grade 485

Suministrada por:

1 proveedor Matmatch

Unclassified Carbon Steel

ASTM A516 Grade 450 As-Rolled or Normalized and/or Stress Relieved

Suministrada por:

1 proveedor Matmatch

Unclassified Carbon Steel

ASTM A516 Grade 485 As-Rolled or Normalized and/or Stress Relieved

Suministrada por:

1 proveedor Matmatch

Unclassified Carbon Steel

ASTM A572 Grade 380

Suministrada por:

1 proveedor Matmatch

Unclassified Carbon Steel

ASTM A572 Grade 345

Suministrada por:

1 proveedor Matmatch