General
Property | Value | Comment |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel |
Elongation | 14.2 % Show Material materials with Elongation of 14.2 % | Predicted Value, A200 |
15.6 % Show Material materials with Elongation of 15.6 % | Predicted Value, A80 | |
18.3 % Show Material materials with Elongation of 18.3 % | Predicted Value, Transverse | |
19.6 % Show Material materials with Elongation of 19.6 % | Predicted Value, A80 Transverse | |
20.3 % Show Material materials with Elongation of 20.3 % | Predicted Value, A5 | |
21.2 % Show Material materials with Elongation of 21.2 % | Predicted Value, A50 | |
21.4 % Show Material materials with Elongation of 21.4 % | Predicted Value | |
Hardness, Brinell | 244 [-] Show Material materials with Hardness, Brinell of 244 [-] | Predicted Value, Transverse |
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel |
Reduction of area | 41.6 % Show Material materials with Reduction of area of 41.6 % | Predicted Value |
43.1 % Show Material materials with Reduction of area of 43.1 % | Predicted Value, Transverse | |
Shear modulus | 79.5 GPa Show Material materials with Shear modulus of 79.5 GPa | Predicted Value |
Shear strength | 515.9 MPa Show Material materials with Shear strength of 515.9 MPa | Predicted Value |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 11.78 1/K Show Material materials with Coefficient of thermal expansion of 11.78 1/K | Predicted Value |
Max service temperature | 299.5 °C Show Material materials with Max service temperature of 299.5 °C | Predicted Value, Long |
Specific heat capacity | 460.9 J/(kg·K) Show Material materials with Specific heat capacity of 460.9 J/(kg·K) | Predicted Value |
Thermal conductivity | 40.51 W/(m·K) Show Material materials with Thermal conductivity of 40.51 W/(m·K) | Predicted Value |
Electrical
Chemical properties
Property | Value | Related Standards |
---|---|---|
Carbon | 0.23 % Show Material materials with Carbon of 0.23 % | ASTM A572 |
Manganese | 1.65 % Show Material materials with Manganese of 1.65 % | ASTM A572 |
Phosphorus | 0.03 % Show Material materials with Phosphorus of 0.03 % | ASTM A572 |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % | ASTM A572 |
Sulfur | 0.03 % Show Material materials with Sulfur of 0.03 % | ASTM A572 |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |