Grey Cast Iron
EN 1561 Grade GJL-300 cast conditionMalleable Cast Iron
SAE J158 Grade M3210 AnnealedMalleable Cast Iron
SAE J158 Grade M4504 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5003 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5503 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M7002 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M8501 Liquid quenched and TemperedMalleable Cast Iron
EN 1562 Grade GJMW-360-12 decarburized annealedPolyamide 12 (PA12)
Polyamide 12 + Metal Powder (PA12+MED)Hierro fundido
EN 1562 Grade GJMB-350-10 not decarburized annealedHierro fundido
EN 1562 Grade GJMB-450-6 not decarburized annealedHierro fundido
EN 1562 Grade GJMB-550-4 not decarburized annealedHierro fundido
EN 1562 Grade GJMB-650-2 not decarburized annealedHierro fundido
EN 1562 Grade GJMB-700-2 not decarburized annealedMalleable Cast Iron
DIN 1692 Grade GTW-40-05 decarburized annealedMalleable Cast Iron
DIN 1692 Grade GTW-45-07 decarburized annealedMalleable Cast Iron
DIN 1692 Grade GTW-S 38-12 decarburized annealedGrey Cast Iron
DIN 1691 Grade GG-30Malleable Cast Iron
DIN 1692 Grade GTW-35-04 decarburized annealedHierro fundido
SAE J434 Grade D4512