Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Wrought Copper High Copper Alloy
ASTM B194 Grade C17200 TD04Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Wrought Copper High Copper Alloy
EN 1652 Grade C17200 TF00Acero inoxidable austenítico
Esshete 1250Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable dúplex
Sandvik SAF 2205™ Solution AnnealedSuministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable dúplex
Sandvik SAF 2205™ Cold WorkedSuministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable ferrítico
DIN 17440 Grade X3CrTi17 soft annealed (+A)Acero inoxidable ferrítico
DIN 17440 Grade X6CrAl13 soft annealed (+A)Acero bajo en carbono
DIN 17175 Grade St 35.8 normalized or normalized formed (+N)Acero inoxidable ferrítico
EN 10088-1 Grade X3CrNb17 soft annealed (+A)Acero bajo en carbono
EN 10216-2 Grade St 45.8 normalized or normalized formed (+N)Acero bajo en carbono
EN 10217-2 Grade St 37.8 normalized or normalized formed (+N)Acero inoxidable ferrítico
SEW 400 Grade X20CrMo13 quenched and tempered (+QT)Acero inoxidable austenítico
EN 10028-7 Grade X8CrNiNb16-13 solution annealed (+AT)Acero inoxidable ferrítico
EN 10088-1 Grade X6CrAl13 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X6CrMo17-1 soft annealed (+A)Acero inoxidable ferrítico
EN 10088-1 Grade X3CrTi17 soft annealed (+A)