Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TH04Nickel Molybdenum Steel
ASTM A387 Grade 11 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedSuministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B768 Grade C17510 TF00Wrought Copper High Copper Alloy
ASTM B251 Grade C17000 TD04Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TF00Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TB00Wrought Copper High Copper Alloy
ASTM B196 Grade C17000 TH04Wrought Copper High Copper Alloy
ASTM B441 Grade C17500 TH04Wrought Copper High Copper Alloy
ASTM B9 Grade C17510 TB00