Acero bajo en carbono
EN 10028-3 Grade P355NL1 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10028-3 Grade P355NL2 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Acero bajo en carbono
EN 10025-3 Grade S355NL normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Medium Carbon Steel
EN 10028-3 Grade P355N normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Nickel Molybdenum Steel
EN 10028-2 Grade 20MnMoNi4-5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 12CrMoV12-10 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoSi5-5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Nickel molybdenum Steel
EN 10028-2 Grade 15NiCuMoNb5-6-4 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
7000 Serie
AA Standards Grade 7075 T7351Unclassified Low Alloy Steel
EN 10028-3 Grade P460NH normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Nickel Steel
EN 10028-4 Grade 13MnNi6-3 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Wrought Copper High Copper Alloy
ASTM B196 Grade C17200 TB00Acero bajo en carbono
ASTM A841 Grade B Class 1 Thermo-Mechanical Control Process (TMCP)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S355M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S355ML thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P355Q quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P355QL1 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-6 Grade P355QL2 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch