Property | Value | Comment |
---|---|---|
Density | 7.8 g/cm³ Show Material materials with Density of 7.8 g/cm³ | Typical for Steel |
Mechanical
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Elastic modulus | 190 - 210 GPa Show Material materials with Elastic modulus of 190 - 210 GPa | Typical for Steel | ||||
Elongation | 17.4 % Show Material materials with Elongation of 17.4 % | Predicted Value, A200 | ||||
17.7 % Show Material materials with Elongation of 17.7 % | Predicted Value, A80 | |||||
19.4 % Show Material materials with Elongation of 19.4 % | Predicted Value, A80 Transverse | |||||
20.5 % Show Material materials with Elongation of 20.5 % | Predicted Value, A5 | |||||
21.5 % Show Material materials with Elongation of 21.5 % | Predicted Value, Transverse | |||||
24.5 % Show Material materials with Elongation of 24.5 % | Predicted Value, A50 | |||||
20 °C | 22 % Show Material materials with Elongation of 22 % | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Poisson's ratio | 0.3 [-] Show Material materials with Poisson's ratio of 0.3 [-] | Typical for Steel | ||||
Reduction of area | 43.3 % Show Material materials with Reduction of area of 43.3 % | Predicted Value | ||||
43.3 % Show Material materials with Reduction of area of 43.3 % | Predicted Value, Transverse | |||||
Shear modulus | 80.3 GPa Show Material materials with Shear modulus of 80.3 GPa | Predicted Value | ||||
Shear strength | 543 MPa Show Material materials with Shear strength of 543 MPa | Predicted Value | ||||
Tensile strength | 20 °C | 450 - 630 MPa Show Material materials with Tensile strength of 450 - 630 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | |
20 °C | 450 - 590 MPa Show Material materials with Tensile strength of 450 - 590 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 490 - 630 MPa Show Material materials with Tensile strength of 490 - 630 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 490 - 590 MPa Show Material materials with Tensile strength of 490 - 590 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
Yield strength | 263.3 MPa Show Material materials with Yield strength of 263.3 MPa | Predicted Value, RP1 | ||||
323.3 MPa Show Material materials with Yield strength of 323.3 MPa | Predicted Value, RP1 Transverse | |||||
370.7 MPa Show Material materials with Yield strength of 370.7 MPa | Predicted Value, RP02 | |||||
374.7 MPa Show Material materials with Yield strength of 374.7 MPa | Predicted Value, Transverse | |||||
429.9 MPa Show Material materials with Yield strength of 429.9 MPa | Predicted Value, RP05 | |||||
472.1 MPa Show Material materials with Yield strength of 472.1 MPa | Predicted Value, RP02 Transverse | |||||
496.6 MPa Show Material materials with Yield strength of 496.6 MPa | Predicted Value, RP002 | |||||
20 °C | 315 MPa Show Material materials with Yield strength of 315 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 335 MPa Show Material materials with Yield strength of 335 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat | ||
20 °C | 355 MPa Show Material materials with Yield strength of 355 MPa | quenched and tempered (+QT) | EN 10028-6 | Flat |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 12.02 1/K Show Material materials with Coefficient of thermal expansion of 12.02 1/K | Predicted Value |
Specific heat capacity | 449.7 J/(kg·K) Show Material materials with Specific heat capacity of 449.7 J/(kg·K) | Predicted Value |
Thermal conductivity | 36.98 W/(m·K) Show Material materials with Thermal conductivity of 36.98 W/(m·K) | Predicted Value |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Boron | 0.005 % Show Material materials with Boron of 0.005 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Carbon | 0.16 % Show Material materials with Carbon of 0.16 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Chromium | 0.3 % Show Material materials with Chromium of 0.3 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Copper | 0.3 % Show Material materials with Copper of 0.3 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Molybdenum | 0.25 % Show Material materials with Molybdenum of 0.25 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Nitrogen | 0.015 % Show Material materials with Nitrogen of 0.015 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Phosphorus | 0.025 % Show Material materials with Phosphorus of 0.025 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Sulfur | 0.01 % Show Material materials with Sulfur of 0.01 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
0.015 % Show Material materials with Sulfur of 0.015 % | quenched and tempered (+QT) | EN 10028-6 | Flat | |
Titanium | 0.03 % Show Material materials with Titanium of 0.03 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Vanadium | 0.06 % Show Material materials with Vanadium of 0.06 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Zirconium | 0.05 % Show Material materials with Zirconium of 0.05 % | quenched and tempered (+QT) | EN 10028-6 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |
Do you have a technical question or need more information about this material?
Post it as a comment below and receive answers from engineers and other community members.