Límite elástico Rp 0,2: 790 - 930 MPa

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Unclassified Low Alloy Steel

EN 10025-6 Grade S960Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Unclassified Low Alloy Steel

ISO 683-2 Grade 33MnCrB5-2 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Nickel Chromium Iron Alloy

VDM® Alloy 718

Suministrada por:

VDM Metals

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TB00

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TH04

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

Wrought Copper High Copper Alloy

ASTM B441 Grade C17500 TH04

Acero inoxidable austenítico

UGI® 209 Solution Annealed

Suministrada por:

Ugitech

Acero inoxidable dúplex

UGIMA® 4460 Cold Finished and Drawn

Suministrada por:

Ugitech

Bronce fosforado

UNS C51900 R850

Acero inoxidable martensítico

UGI 4418 QT900 Turned Bar

Suministrada por:

Ugitech

Acero inoxidable martensítico

UGI 4418 AIR QT1100

Suministrada por:

Ugitech

Acero inoxidable martensítico

UGI 4418 AIR QT1150

Suministrada por:

Ugitech

Acero inoxidable endurecido por precipitación

UGI® 4545 AIR H1075

Suministrada por:

Ugitech
Página 1 de 12