General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 3.8 % Show Supplier Material materials with Absorción de agua of 3.8 % | dry | ISO 62 | at 23°C after 24h |
13.5 % Show Supplier Material materials with Absorción de agua of 13.5 % | dry | Sim. to ISO 62 | ||
Densidad | 1.18 g/cm³ Show Supplier Material materials with Densidad of 1.18 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3.7 % Show Supplier Material materials with Moisture absorption of 3.7 % | dry | Sim. to ISO 62 | |
Índice límite de óxigeno | 27 % Show Supplier Material materials with Índice límite de óxigeno of 27 % | dry | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | -40 °C | 20 % Show Supplier Material materials with Elongación of 20 % | dry | ISO 527-1/-2 |
40 % Show Supplier Material materials with Elongación of 40 % | dry | ISO 527-1/-2 | ||
50 % Show Supplier Material materials with Elongación of 50 % | conditioned | ISO 527-1/-2 | ||
120 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
160 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
180 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
200 °C | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongation at yield of 20 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 50 MPa Show Supplier Material materials with Flexural yield strength of 50 MPa | conditioned | ISO 178 | |
150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | ||
120 °C | 50 MPa Show Supplier Material materials with Flexural yield strength of 50 MPa | dry | ISO 178 | |
160 °C | 40 MPa Show Supplier Material materials with Flexural yield strength of 40 MPa | dry | ISO 178 | |
Límite elástico | -40 °C | 135 MPa Show Supplier Material materials with Límite elástico of 135 MPa | dry | ISO 527-1/-2 |
55.0 MPa Show Supplier Material materials with Límite elástico of 55.0 MPa | conditioned | ISO 527-1/-2 | ||
100 MPa Show Supplier Material materials with Límite elástico of 100 MPa | dry | ISO 527-1/-2 | ||
120 °C | 50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | dry | ISO 527-1/-2 | |
160 °C | 40 MPa Show Supplier Material materials with Límite elástico of 40 MPa | dry | ISO 527-1/-2 | |
180 °C | 35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | dry | ISO 527-1/-2 | |
200 °C | 30 MPa Show Supplier Material materials with Límite elástico of 30 MPa | dry | ISO 527-1/-2 | |
Módulo de flexión | 0.9 GPa Show Supplier Material materials with Módulo de flexión of 0.9 GPa | conditioned | ISO 178 | |
3 GPa Show Supplier Material materials with Módulo de flexión of 3 GPa | dry | ISO 178 | ||
120 °C | 0.8 GPa Show Supplier Material materials with Módulo de flexión of 0.8 GPa | dry | ISO 178 | |
160 °C | 0.6 GPa Show Supplier Material materials with Módulo de flexión of 0.6 GPa | dry | ISO 178 | |
Módulo elástico | -40 °C | 3.3 GPa Show Supplier Material materials with Módulo elástico of 3.3 GPa | dry | ISO 527-1/-2 |
1 GPa Show Supplier Material materials with Módulo elástico of 1 GPa | conditioned | ISO 527-1/-2 | ||
3.3 GPa Show Supplier Material materials with Módulo elástico of 3.3 GPa | dry | ISO 527-1/-2 | ||
120 °C | 0.8 GPa Show Supplier Material materials with Módulo elástico of 0.8 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.65 GPa Show Supplier Material materials with Módulo elástico of 0.65 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.6 GPa Show Supplier Material materials with Módulo elástico of 0.6 GPa | dry | ISO 527-1/-2 | |
200 °C | 0.5 GPa Show Supplier Material materials with Módulo elástico of 0.5 GPa | dry | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 4 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | dry | ISO 179/1eA | |
23 °C | 35 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 35 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 8.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.1e-06 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Difusividad térmica | 9.21e-08 mm²/s Show Supplier Material materials with Difusividad térmica of 9.21e-08 mm²/s | dry | - | |||
Glow Wire Flammability Index | 650 °C Show Supplier Material materials with Glow Wire Flammability Index of 650 °C | dry | IEC 60695-2-12 | 3 mm | ||
750 °C Show Supplier Material materials with Glow Wire Flammability Index of 750 °C | dry | IEC 60695-2-12 | 0.75 mm | |||
Glow Wire Ignition Temperature | 700 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 700 °C | dry | IEC 60695-2-13 | 3 mm | ||
725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | dry | IEC 60695-2-13 | 0.75 mm | |||
Inflamabilidad | V-2 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 115 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 115 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | dry | UL746B | 0.75 mm | ||
Temperatura de flexión bajo carga | 190 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
280 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 280 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de reblandecimiento Vicat | 290 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 290 °C | dry | ISO 306 | 50°C/h 50N | ||
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.6 [-] | dry | IEC 62631-2-1 | 1MHz |
3.9 [-] Show Supplier Material materials with Constante dieléctrica of 3.9 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.5 [-] Show Supplier Material materials with Constante dieléctrica of 4.5 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
22 [-] Show Supplier Material materials with Constante dieléctrica of 22 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Factor de disipación | 70 [-] Show Supplier Material materials with Factor de disipación of 70 [-] | dry | IEC 62631-2-1 | 100Hz |
260 [-] Show Supplier Material materials with Factor de disipación of 260 [-] | dry | IEC 62631-2-1 | 1MHz | |
1200 [-] Show Supplier Material materials with Factor de disipación of 1200 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
8700 [-] Show Supplier Material materials with Factor de disipación of 8700 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Rigidez dieléctrica | 15 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 15 kV/mm | conditioned | IEC 60243-1 | |
25 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 25 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 1e+07 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+07 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 400 V Show Supplier Material materials with Índice de seguimiento comparativo of 400 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Parallel |
2 % Show Supplier Material materials with Contracción of 2 % | dry | Sim. to ISO 294-4 | Normal | |
Density of melt | 990 g/cm³ Show Supplier Material materials with Density of melt of 990 g/cm³ | dry | - | |
Specific heat capacity melt | 2670 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2670 J/(kg·K) | dry | - | |
Spiral flow length | 110 | dry | - | 1.0 mm 800 bar |
120 | dry | - | 1.0 mm 900 bar | |
130 | dry | - | 1.0 mm 1000 bar | |
60 | dry | - | 0.5mm 1200 bar | |
70 | dry | - | 0.5mm 1600 bar | |
90 | dry | - | 0.5mm 2000 bar | |
Thermal conductivity of melt | 0.25 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.25 W/(m·K) | dry | - | |
Viscosity number | 185 cm³/gr Show Supplier Material materials with Viscosity number of 185 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Small domestic appliance gears, Variator transmission parts, Ironing Components, Golf Shoe Receptacles, Chain Tensioners, Variator Roller Cover, Transmission Control Gears, Bike Body Plugs, Oil Pump Gears (2-wheelers), Slide Shoe Surfaces in new generation, MTF/DMF Components, CVT Transmission Systems: Scoop Snubbers, Crankshaft Balance Gears, EPS gears, Power Lift Gate Actuators, Power Door Actuators, Power Window Actuators, Windshield Wiper Actuators, Power Seats, EPS Steering components: Gears, Flex couplers and Sensors, Fuel System: Various Components, Automotive Connectors, Endlaminates (electro motors), Brushholders (electro motors), Coil insulation, Automotive e-motor Bobbins, Temperature Sensor, Speed Sensor, Positition Sensor, Start/Stop: Alternator and Starter parts, Endlaminates (electrical components), Brushholders (electrical components), Cable Ties, Door checker, Gears, Timing drive systems, Electric parking brakes, Electric brake boosters, Seat actuators, Mirror actuators, Trunk actuators, Door handle actuators, Sunroof actuators, Steering wheel adjusters | |
Certifications | Yellow Card Available |