Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.57 g/cm³ Show Supplier Material materials with Densidad of 1.57 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 2.5 % Show Supplier Material materials with Elongación of 2.5 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Elongación of 5 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 275 MPa Show Supplier Material materials with Flexural yield strength of 275 MPa | conditioned | ISO 178 | |
335 MPa Show Supplier Material materials with Flexural yield strength of 335 MPa | dry | ISO 178 | ||
Módulo de flexión | 12 GPa Show Supplier Material materials with Módulo de flexión of 12 GPa | conditioned | ISO 178 | |
14.5 GPa Show Supplier Material materials with Módulo de flexión of 14.5 GPa | dry | ISO 178 | ||
Módulo elástico | 12.5 GPa Show Supplier Material materials with Módulo elástico of 12.5 GPa | conditioned | ISO 527-1/-2 | |
16.5 GPa Show Supplier Material materials with Módulo elástico of 16.5 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 165 MPa Show Supplier Material materials with Resistencia a la tracción of 165 MPa | conditioned | ISO 527-1/-2 | |
220 MPa Show Supplier Material materials with Resistencia a la tracción of 220 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | dry | ISO 179/1eA | |
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | conditioned | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 1.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Inflamabilidad | HB | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Temperatura de flexión bajo carga | 200 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 200 °C | dry | ISO 75-1/-2 | 2 MPa | ||
215 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 21 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 21 kV/mm | conditioned | IEC 60243-1 |
23 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 23 kV/mm | dry | IEC 60243-1 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Índice de seguimiento comparativo | 450 V Show Supplier Material materials with Índice de seguimiento comparativo of 450 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | HVAC lamellae | |
Certifications | Yellow Card Available | |
Fillers | 50% Glass Fiber |