EN 573-3 Grade AW-6262 T8

Want to keep this datasheet? Save it now in your required format

Description

EN AW-6262 is a free-machining alloy that offers users outstanding mechanical strength and good resistance to corrosion. Aluminum EN AW-6262 is heat treatable and due to the addition of bismuth is easily machinable. Anodizing raises the levels of corrosion resistance and with high-speed tooling you can achieve a smooth finish. Welding of Aluminum EN AW-6262 is achieved through gas, arc, and resistance methods. The most common tempers of EN AW-6262 are T6 and T9.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.72 g/cm³

Show Material materials with Density of 2.72 g/cm³

T8

EN 573-3, EN 754

Rod, Tube

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

T8

EN 573-3, EN 754

Rod, Tube

Elongation

20.0 °C

3.0 %

Show Material materials with Elongation of 3.0 %

T8

EN 573-3

Rod, Tube

A50

3.0 %

Show Material materials with Elongation of 3.0 %

T8

EN 573-3, EN 754

Rod, Tube

A50

20.0 °C

4.0 %

Show Material materials with Elongation of 4.0 %

T8

EN 573-3

Rod, Tube

4.0 %

Show Material materials with Elongation of 4.0 %

T8

EN 573-3, EN 754

Rod, Tube

A100

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 6000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 6000 Series Aluminium

Shear modulus

26.0 - 26.5 GPa

Show Material materials with Shear modulus of 26.0 - 26.5 GPa

Typical for Wrought 6000 Series Aluminium

Tensile strength

20.0 °C

345.0 MPa

Show Material materials with Tensile strength of 345.0 MPa

T8

EN 573-3

Rod, Tube

345.0 MPa

Show Material materials with Tensile strength of 345.0 MPa

T8

EN 573-3, EN 754

Rod, Tube

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.6e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.4e-05 1/K

Typical for Wrought 6000 Series Aluminium

Melting point

555.0 - 655.0 °C

Show Material materials with Melting point of 555.0 - 655.0 °C

Typical for Wrought 6000 Series Aluminium

Specific heat capacity

887.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 887.0 - 963.0 J/(kg·K)

Typical for Wrought 6000 Series Aluminium

Thermal conductivity

170.0 - 220.0 W/(m·K)

Show Material materials with Thermal conductivity of 170.0 - 220.0 W/(m·K)

Typical for Wrought 6000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

21000000.0 - 34000000.0 S/m

Show Material materials with Electrical conductivity of 21000000.0 - 34000000.0 S/m

Typical for Wrought 6000 Series Aluminium

Electrical resistivity

2.9e-08 - 5e-08 Ω·m

Show Material materials with Electrical resistivity of 2.9e-08 - 5e-08 Ω·m

Typical for Wrought 6000 Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Bismuth

0.4 - 0.7 %

Show Material materials with Bismuth of 0.4 - 0.7 %

T8

EN 573-3, EN 754

Rod, Tube

Chromium

0.04 - 0.14 %

Show Material materials with Chromium of 0.04 - 0.14 %

T8

EN 573-3, EN 754

Rod, Tube

Copper

0.15 - 0.4 %

Show Material materials with Copper of 0.15 - 0.4 %

T8

EN 573-3, EN 754

Rod, Tube

Iron

0.7 %

Show Material materials with Iron of 0.7 %

T8

EN 573-3

Rod, Tube

0.70 %

Show Material materials with Iron of 0.70 %

T8

EN 573-3, EN 754

Rod, Tube

Lead

0.4 - 0.7 %

Show Material materials with Lead of 0.4 - 0.7 %

T8

EN 573-3, EN 754

Rod, Tube

Magnesium

0.8 - 1.2 %

Show Material materials with Magnesium of 0.8 - 1.2 %

T8

EN 573-3, EN 754

Rod, Tube

Manganese

0.15 %

Show Material materials with Manganese of 0.15 %

T8

EN 573-3, EN 754

Rod, Tube

Silicon

0.4 - 0.8 %

Show Material materials with Silicon of 0.4 - 0.8 %

T8

EN 573-3, EN 754

Rod, Tube

Titanium

0.15 %

Show Material materials with Titanium of 0.15 %

T8

EN 573-3, EN 754

Rod, Tube

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

T8

EN 573-3, EN 754

Rod, Tube

Technological properties

Property
Workability

Excellent workability.