General
Property | Value | Condition | Related Standards |
---|---|---|---|
Density | 2.82 g/cm³ Show Material materials with Density of 2.82 g/cm³ | H13 | EN 573-3, EN 1301 |
2.83 g/cm³ Show Material materials with Density of 2.83 g/cm³ | H13 | EN 573-3, EN 1301 |
Mechanical
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Elastic modulus | 70.0 GPa Show Material materials with Elastic modulus of 70.0 GPa | H13 | EN 573-3, EN 1301 | |
72.5 GPa Show Material materials with Elastic modulus of 72.5 GPa | H13 | EN 573-3, EN 1301 | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||
Shear modulus | 27.3 GPa Show Material materials with Shear modulus of 27.3 GPa | H13 | EN 573-3, EN 1301 | |
Tensile strength | 155.0 - 225.0 MPa Show Material materials with Tensile strength of 155.0 - 225.0 MPa | H13 | EN 573-3, EN 1301 |
Thermal
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Coefficient of thermal expansion | -50 °C | 2.14e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.14e-05 1/K | H13 | EN 573-3, EN 1301 |
20 °C | 2.14e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.14e-05 1/K | H13 | EN 573-3, EN 1301 | |
20 °C | 2.2899999999999998e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2899999999999998e-05 1/K | H13 | EN 573-3, EN 1301 | |
20 °C | 2.3399999999999996e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K | H13 | EN 573-3, EN 1301 | |
20 °C | 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K | H13 | EN 573-3, EN 1301 | |
20 °C | 2.4999999999999998e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.4999999999999998e-05 1/K | H13 | EN 573-3, EN 1301 | |
100 °C | 2.2899999999999998e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2899999999999998e-05 1/K | H13 | EN 573-3, EN 1301 | |
100 °C | 2.3399999999999996e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3399999999999996e-05 1/K | H13 | EN 573-3, EN 1301 | |
200 °C | 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K | H13 | EN 573-3, EN 1301 | |
300 °C | 2.4999999999999998e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.4999999999999998e-05 1/K | H13 | EN 573-3, EN 1301 | |
Melting point | 540.0 - 645.0 °C Show Material materials with Melting point of 540.0 - 645.0 °C | H13 | EN 573-3, EN 1301 | |
585.0 - 650.0 °C Show Material materials with Melting point of 585.0 - 650.0 °C | H13 | EN 573-3, EN 1301 | ||
Specific heat capacity | 864.0 J/(kg·K) Show Material materials with Specific heat capacity of 864.0 J/(kg·K) | H13 | EN 573-3, EN 1301 | |
Thermal conductivity | 151.0 - 172.0 W/(m·K) Show Material materials with Thermal conductivity of 151.0 - 172.0 W/(m·K) | H13 | EN 573-3, EN 1301 | |
170.0 - 220.0 W/(m·K) Show Material materials with Thermal conductivity of 170.0 - 220.0 W/(m·K) | H13 | EN 573-3, EN 1301 |
Electrical
Property | Value | Condition | Related Standards |
---|---|---|---|
Electrical conductivity | 23000000.0 - 26000000.0 S/m Show Material materials with Electrical conductivity of 23000000.0 - 26000000.0 S/m | H13 | EN 573-3, EN 1301 |
24000000.0 - 32000000.0 S/m Show Material materials with Electrical conductivity of 24000000.0 - 32000000.0 S/m | H13 | EN 573-3, EN 1301 | |
Electrical resistivity | 3.13e-08 - 4.17e-08 Ω·m Show Material materials with Electrical resistivity of 3.13e-08 - 4.17e-08 Ω·m | H13 | EN 573-3, EN 1301 |
3.85e-08 - 4.35e-08 Ω·m Show Material materials with Electrical resistivity of 3.85e-08 - 4.35e-08 Ω·m | H13 | EN 573-3, EN 1301 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Bismuth | 0.2 - 0.8 % Show Material materials with Bismuth of 0.2 - 0.8 % | H13 | EN 573-3, EN 1301 |
Copper | 5.0 - 6.0 % Show Material materials with Copper of 5.0 - 6.0 % | H13 | EN 573-3, EN 1301 |
Iron | 0.70 % Show Material materials with Iron of 0.70 % | H13 | EN 573-3, EN 1301 |
Lead | 0.2 - 0.6 % Show Material materials with Lead of 0.2 - 0.6 % | H13 | EN 573-3, EN 1301 |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % | H13 | EN 573-3, EN 1301 |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % | H13 | EN 573-3, EN 1301 |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not suitable, Protective: poor | |
Brazing | hard brazing (with flux/ without flux): not suitable /, friction soldering: sufficient | |
Corrosion properties | Seawater: poor, weathering: sufficient | |
Workability | Deep drawing / upsetting (Condition) - / acceptable |