Polyethylene Terephthalate (PET) Granule (ES306312)

Alternative and trade names
Polyethylene Terephthalate (PET) Granule (ES306312)
.XLSX
.PDF
Save

Description

Polyethylene Terephthalate granules have cylindrical shape. It is a food grade copolymer fast reheat resin engineered to deliver the most efficient injection moulding and blowing while maintaining excellent colour characteristics. It builds upon the established combination of slow crystallisation at moulding and reduced energy consumption at blowing which results in energy and cycle time reduction versus conventional resins. It is also suitable for conversion into extruded sheet and thermoformed containers.

Properties

General

Bulk density ρbulk

0.84 g/cm³ at 20 °C

Crystallinity ccryst

48 % at 20 °C

measured by density

Density ρ

1.39 g/cm³ at 20 °C

absolute

Particle mass mpart

19 mg at 20 °C

Water absorption cwater

0.2 % at 20 °C

Thermal

Glass transition temperature Tg

83 °C

Melting point Tm

248 °C

Technological properties

Processing methods

Blow molding, injection molding, sheet extrusion, thermoforming

This material data has been provided by Goodfellow.