PropertyValue

Dimensions

Briquette size: 18 x 12 x 7 mm approx. (0.75 x 0.5 x 0.25 inches approx.), pillow shaped

Chemical properties

PropertyValueComment

Carbon

5E-3 %

Show Supplier Material materials with Carbon of 5E-3 %

max

Nitrogen

0.01 %

Show Supplier Material materials with Nitrogen of 0.01 %

max

Other

0.01 %

Show Supplier Material materials with Other of 0.01 %

total metallic impurities max.

Oxygen

0.06 %

Show Supplier Material materials with Oxygen of 0.06 %

max

Rhenium

balance

Sulfur

3E-3 %

Show Supplier Material materials with Sulfur of 3E-3 %

max

Technological properties

Property
Application areas

Common uses: As an addition to superalloys for components in high temperature sectors of aerospace and power generation turbines

Processing history

Produced by sintering rhenium metal powder