Ammonium Perrhenate

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Molymet.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValueComment

Other

0.01 %

Show Supplier Material materials with Other of 0.01 %

total metallic impurities max.

Rhenium

69.4 %

Show Supplier Material materials with Rhenium of 69.4 %

Technological properties

Property
Application areas

Common uses: Manufacture of bimetallic Pt/Re reforming catalysts, production of rhenium metal and production of perrhenic acid

Color

White crystaline powder

Processing history

Recovered as a by-product of molybdenum concentrates processing