Rhenium Metal Powder (min. 99.97% Purity)

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Molymet.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Particle size

63000 nm

Show Supplier Material materials with Particle size of 63000 nm

Sieve analysis from 270 mesh to 100 mesh (typical max value, others as requested)

Particle size range

3.5 - 4 µm

Show Supplier Material materials with Particle size range of 3.5 - 4 µm

Fisher S.S.S. (typical value, others as requested)

Chemical properties

PropertyValueComment

Carbon

5E-3 %

Show Supplier Material materials with Carbon of 5E-3 %

max

Nitrogen

0.01 %

Show Supplier Material materials with Nitrogen of 0.01 %

max

Other

0.02 %

Show Supplier Material materials with Other of 0.02 %

total metallic impurities max.

Oxygen

0.25 %

Show Supplier Material materials with Oxygen of 0.25 %

max

Rhenium

balance

Sulfur

3E-3 %

Show Supplier Material materials with Sulfur of 3E-3 %

max

Technological properties

Property
Application areas

Common uses: As an alloy addition in superalloys; production of sheet foil, strip or wire for various industrial applications

Processing history

Produced by hydrogen reduction of Ammonium Perrhenate