The material: 'Melted Quality Tantalum (TaM) Pickled Rod 6 mm' you were looking for has been superseded by the one below.

Melted Quality Tantalum (TaM) Pickled Rod

Want to keep this datasheet? Save it now in your required format

Description

Melted quality tantalum (TaM) is usually more economical to produce than sintered quality tantalum and provides sufficient quality for many applications. However, the material is neither as fine nor as homogeneous as sintered quality tantalum.

This material data has been provided by Plansee.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

16.6 g/cm³

Show Supplier Material materials with Density of 16.6 g/cm³

Neutron capture cross-section

23.0 °C

0 m²

Show Supplier Material materials with Neutron capture cross-section of 0 m²

Dimension

PropertyValue

Diameter

4 - 10 mm

Show Supplier Material materials with Diameter of 4 - 10 mm

Length

300 - 2500 mm

Show Supplier Material materials with Length of 300 - 2500 mm

Dimensions

Available dimensions (diameter x length, mm x mm): 4 x 500-2000 ; 6 x 500-2500 ; 10 x 300-2500

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

25 %

Show Supplier Material materials with Elongation of 25 %

Tensile strength

23.0 °C

172 MPa

Show Supplier Material materials with Tensile strength of 172 MPa

Yield strength Rp0.2

23.0 °C

103 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 103 MPa

Thermal

PropertyValue

Crystallization temperature

900 - 1450 °C

Show Supplier Material materials with Crystallization temperature of 900 - 1450 °C

Melting point

2966 °C

Show Supplier Material materials with Melting point of 2966 °C

Electrical

PropertyTemperatureValue

Electron work function

23.0 °C

4.3 eV

Show Supplier Material materials with Electron work function of 4.3 eV

Superconductive transition temperature

-268.65 °C

Show Supplier Material materials with Superconductive transition temperature of -268.65 °C

Acoustical

PropertyTemperatureValue

Sound speed, longitudinal

23.0 °C

4100 m/s

Show Supplier Material materials with Sound speed, longitudinal of 4100 m/s

Sound speed, transversal

23.0 °C

2900 m/s

Show Supplier Material materials with Sound speed, transversal of 2900 m/s

Chemical properties

PropertyValueComment

Cadmium

1E-4 %

Show Supplier Material materials with Cadmium of 1E-4 %

Carbon

1E-3 %

Show Supplier Material materials with Carbon of 1E-3 %

Hydrogen

4E-4 %

Show Supplier Material materials with Hydrogen of 4E-4 %

Iron

5E-4 %

Show Supplier Material materials with Iron of 5E-4 %

Molybdenum

1E-3 %

Show Supplier Material materials with Molybdenum of 1E-3 %

Nickel

5E-4 %

Show Supplier Material materials with Nickel of 5E-4 %

Niobium

1.9E-3 %

Show Supplier Material materials with Niobium of 1.9E-3 %

Nitrogen

5E-4 %

Show Supplier Material materials with Nitrogen of 5E-4 %

Oxygen

1.3E-3 %

Show Supplier Material materials with Oxygen of 1.3E-3 %

Silicon

1E-3 %

Show Supplier Material materials with Silicon of 1E-3 %

Tantalum

99.95 %

Show Supplier Material materials with Tantalum of 99.95 %

min

Titanium

1E-4 %

Show Supplier Material materials with Titanium of 1E-4 %

Tungsten

2E-3 %

Show Supplier Material materials with Tungsten of 2E-3 %

Technological properties

Property
Corrosion properties

Outstanding resistance against aqueous solutions and metal melts.

Other

This material has excellent cold ductility, superconductivity and a high level of biocompatibility.