Tungsten Lanthanum Oxide (WL10) Ground Rod

Want to keep this datasheet? Save it now in your required format

Description

Tungsten is doped with between 1.0 and 2.0 percent of lanthanum oxide (La₂O₃) by weight in order to improve its creep resistance and increase the recrystallization temperature. WL is also easier to machine due to the finely distributed oxide particles in its structure. The electron work function of tungsten-lanthanum oxide is significantly lower than that of pure tungsten.

This material data has been provided by Plansee.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

18.75 - 18.85 g/cm³

Show Supplier Material materials with Density of 18.75 - 18.85 g/cm³

Surface roughness

1 μm

Show Supplier Material materials with Surface roughness of 1 μm

Dimension

PropertyValue

Diameter

3.5 - 20 mm

Show Supplier Material materials with Diameter of 3.5 - 20 mm

Length

300 - 1600 mm

Show Supplier Material materials with Length of 300 - 1600 mm

Dimensions

Available dimensions (diameter x length, mm x mm): 3.5 x 500-1524; 4.5 x 500-1524; 5.5 x 500-1524; 6.5 x 500-1524; 7 x 500-1524; 7.5 x 500-1524; 8.5 x 500-1524; 12.7 x 300-1524; 20 x 300-1600

Mechanical

PropertyTemperatureValue

Hardness, Vickers, 30

23.0 °C

400 - 420 [-]

Show Supplier Material materials with Hardness, Vickers, 30 of 400 - 420 [-]

Chemical properties

PropertyValueComment

Aluminium

1E-4 %

Show Supplier Material materials with Aluminium of 1E-4 %

Cadmium

1E-4 %

Show Supplier Material materials with Cadmium of 1E-4 %

Carbon

6E-4 %

Show Supplier Material materials with Carbon of 6E-4 %

Chromium

3E-4 %

Show Supplier Material materials with Chromium of 3E-4 %

Copper

1E-4 %

Show Supplier Material materials with Copper of 1E-4 %

Iron

8E-4 %

Show Supplier Material materials with Iron of 8E-4 %

Lanthanum

0.77 - 0.94 %

Show Supplier Material materials with Lanthanum of 0.77 - 0.94 %

as La

Lead

1E-4 %

Show Supplier Material materials with Lead of 1E-4 %

Molybdenum

1.2E-3 %

Show Supplier Material materials with Molybdenum of 1.2E-3 %

Nickel

2E-4 %

Show Supplier Material materials with Nickel of 2E-4 %

Nitrogen

1E-4 %

Show Supplier Material materials with Nitrogen of 1E-4 %

Other

0.9 - 1.1 %

Show Supplier Material materials with Other of 0.9 - 1.1 %

as La₂O₃

Potassium

1E-4 %

Show Supplier Material materials with Potassium of 1E-4 %

Silicon

1E-4 %

Show Supplier Material materials with Silicon of 1E-4 %

Tungsten

balance

Technological properties

Property
Application areas

WL is a popular choice for ion sources, lamp electrodes and welding electrodes.