Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 19.2 g/cm³ Show Supplier Material materials with Density of 19.2 g/cm³ |
Neutron capture cross-section | 23.0 °C | 0 m² Show Supplier Material materials with Neutron capture cross-section of 0 m² |
Dimension
Property | Value |
---|---|
Length | 620 - 1000 mm Show Supplier Material materials with Length of 620 - 1000 mm |
Thickness | 0.5 - 5 mm Show Supplier Material materials with Thickness of 0.5 - 5 mm |
Width | 400 - 500 mm Show Supplier Material materials with Width of 400 - 500 mm |
Dimensions | Available dimensions (width x length x thickness, mm x mm x mm): 500 x 1000 x 0.5; 500 x 1000 x 1; 500 x 1000 x 1.5; 500 x 1000 x 2; 400 x 1040 x 3; 400 x 780 x 4; 400 x 620 x 5 |
Mechanical
Property | Temperature | Value |
---|---|---|
Hardness, Vickers | 23.0 °C | 500 [-] Show Supplier Material materials with Hardness, Vickers of 500 [-] |
Thermal
Property | Value |
---|---|
Melting point | 3420 °C Show Supplier Material materials with Melting point of 3420 °C |
Electrical
Property | Temperature | Value |
---|---|---|
Electron work function | 23.0 °C | 4.54 eV Show Supplier Material materials with Electron work function of 4.54 eV |
Acoustical
Chemical properties
Property | Value |
---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % |
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % |
Carbon | 6E-4 % Show Supplier Material materials with Carbon of 6E-4 % |
Chromium | 3E-4 % Show Supplier Material materials with Chromium of 3E-4 % |
Copper | 1E-4 % Show Supplier Material materials with Copper of 1E-4 % |
Iron | 8E-4 % Show Supplier Material materials with Iron of 8E-4 % |
Lead | 1E-4 % Show Supplier Material materials with Lead of 1E-4 % |
Molybdenum | 1.2E-3 % Show Supplier Material materials with Molybdenum of 1.2E-3 % |
Nickel | 2E-4 % Show Supplier Material materials with Nickel of 2E-4 % |
Oxygen | 2E-4 % Show Supplier Material materials with Oxygen of 2E-4 % |
Potassium | 1E-4 % Show Supplier Material materials with Potassium of 1E-4 % |
Silicon | 1E-4 % Show Supplier Material materials with Silicon of 1E-4 % |
Tungsten | 99.97 % Show Supplier Material materials with Tungsten of 99.97 % |