HERAMID A NER MP/1 K

Alternative and trade names
PA66-IT
Want to keep this datasheet? Save it now in your required format

Description

PA66 injection moulding grade. Toughened, heat stabilized. Black colour.

Post-industrial grade produced with selected polymers coming from polymerization, fibres and compounding plants.

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.12 g/cm³

Show Supplier Material materials with Density of 1.12 g/cm³

ISO 1183, DAM

Moisture absorption

23.0 °C

2.5 %

Show Supplier Material materials with Moisture absorption of 2.5 %

ISO 62, 50% RH, thickness tested (mm): 2

Water absorption

23.0 °C

7.5 %

Show Supplier Material materials with Water absorption of 7.5 %

ISO 62, thickness tested (mm): 2

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.4 GPa

Show Supplier Material materials with Elastic modulus of 2.4 GPa

ISO 527-2/1A, 1mm/min, DAM

Elongation

23.0 °C

33 %

Show Supplier Material materials with Elongation of 33 %

ISO 527-2/1A, 50mm/min, DAM

Elongation at yield

23.0 °C

6 %

Show Supplier Material materials with Elongation at yield of 6 %

ISO 527-2/1A, DAM

Flexural modulus

23.0 °C

2.2 GPa

Show Supplier Material materials with Flexural modulus of 2.2 GPa

ISO 178, 2mm/min, DAM

Flexural strength

23.0 °C

90 MPa

Show Supplier Material materials with Flexural strength of 90 MPa

ISO 178, 2mm/min, DAM

Impact strength, Charpy notched

23.0 °C

13 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 13 kJ/m²

ISO 179/1eA

Tensile strength

23.0 °C

60 MPa

Show Supplier Material materials with Tensile strength of 60 MPa

ISO 527-2/1A, 50mm/min, DAM

Yield strength

23.0 °C

60 MPa

Show Supplier Material materials with Yield strength of 60 MPa

ISO 527-2/1A, 50mm/min, DAM

Impact strength, Charpy unnotched

ISO 179/1eU, No Break @ 23°C

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

175 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 175 °C

ISO 75/2Bf

Heat deflection temperature, 1.80 MPa

65 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 65 °C

ISO 75/2Af

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

ISO 11357-1/-3, 10°C/min

Flammability

Automotive Interior Flammability(mm/min): <100 ,method: ISO 3795 and thickness tested (mm): 3 | Class: HB ,method: UL 94, and thickness tested (mm): 0.8

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

8 g/10min

Show Supplier Material materials with Melt mass-flow rate of 8 g/10min

ISO 1133, 275°C/1Kg

Shrinkage

23.0 °C

1.4 %

Show Supplier Material materials with Shrinkage of 1.4 %

ISO 294-4, DAM

Shrinkage, transverse

23.0 °C

1.5 %

Show Supplier Material materials with Shrinkage, transverse of 1.5 %

ISO 294-4, DAM

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Black

Processing methods

Injection Molding