HERAMID S NER GF030/2K

Alternative and trade names
PA6-GF30
Want to keep this datasheet? Save it now in your required format

Description

PA6 30% glass fibre reinforced injection moulding grade. Heat stabilized. Black colour.

Post-industrial grade produced with selected polymers coming from polymerization, fibres and compounding plants.

This material data has been provided by Radici Group.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.37 g/cm³

Show Supplier Material materials with Density of 1.37 g/cm³

ISO 1183, DAM

Water absorption

ISO 62, thickness tested (mm): 2

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

8 GPa

Show Supplier Material materials with Elastic modulus of 8 GPa

ISO 527-2/1A, 1mm/min, DAM

Elongation

23.0 °C

2.7 %

Show Supplier Material materials with Elongation of 2.7 %

ISO 527-2/1A, 5mm/min, DAM

Flexural modulus

23.0 °C

7.3 GPa

Show Supplier Material materials with Flexural modulus of 7.3 GPa

ISO 178, 2mm/min, DAM

Flexural strength

23.0 °C

200 MPa

Show Supplier Material materials with Flexural strength of 200 MPa

ISO 178, 2mm/min, DAM

Impact strength, Charpy notched

23.0 °C

7 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

23.0 °C

60 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

ISO 179/1eU

Tensile strength

23.0 °C

130 MPa

Show Supplier Material materials with Tensile strength of 130 MPa

ISO 527-2/1A, 5mm/min, DAM

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

190 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 190 °C

ISO 75/2Af

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

ISO 11357-1/-3, 10°C/min

Flammability

Class: HB ,method: UL 94, and thickness tested (mm): 0.8

Technological properties

Property
Certifications

RoHS 2011/65/UE

Color

Black

Fillers

30% Glass Fiber

Processing methods

Injection Molding