ALLOW™ Wire Rod Grade A1370 H11

Want to keep this datasheet? Save it now in your required format

Description

Low Carbon Wire Rod ALLOW™ produced with renewable hydropower by RUSAL.

Related Standards

Equivalent Materials

This material data has been provided by Rusal.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Carbon Footprint

Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al.

Dimension

PropertyValue

Dimensions

9,5 mm, 12 mm, 15 mm, 19 mm, 25 mm

Mechanical

PropertyValueTemperature

Tensile strength

80 - 95 MPa

Show Supplier Material materials with Tensile strength of 80 - 95 MPa at 23.0 °C

23.0 °C

Thermal

PropertyValueComment

Melting point

660 °C

Show Supplier Material materials with Melting point of 660 °C

approximate

Electrical

PropertyValueComment

Specific Electrical conductivity

61.9 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 61.9 % IACS

min

Chemical properties

Property

Aluminium

Balance

Iron

0.25 %

Silicon

0.1 %

Technological properties

Property
Application areas

Electric conductors and cables, multi-void conform extrusions

Processing history

Smelters: Irkutsk Aluminium Smelter (IrKAZ), Kandalaksha Aluminium Smelter (KAZ), Bratsk Aluminium Smelter (BrAZ)