Low Carbon Billets ALLOW™ produced with renewable hydropower by RUSAL.
Carbon Footprint
Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al.
Dimensions
Diameter = 152 mm (6”), 178 mm (7”), 203 mm (8”), 228 mm (9”), 254 mm (10”), 279 mm (11”), 306 mm (12”), 356 mm (14”), 406 mm (16”), 457 mm (18”).
Length
l400 - 7000 mm
Melting point
Tm607 - 657 °C
Solidus (607-619°C); Liquidus (655-657°C)
Element
Weight %
Comment
-
Balance
0.6 - 0.9 %
according to EN 573-3
0.4 - 0.6 %
according to EN 573-3
0.35 %
according to EN 573-3
0.15 %
according to EN 573-3
Application areas
Extrusion Applications
Processing history
Smelters: Sayanogorsk Aluminium Smelter (SAZ), Krasnoyarsk Aluminium Smelter (KRAZ), Kubikenborg Aluminium AB (KUBAL)
This material data has been provided by Rusal.