ALLOW™ Wire Rod Grade TAL (AT1)

Want to keep this datasheet? Save it now in your required format

Description

Low Carbon Wire Rod ALLOW™ produced with renewable hydropower by RUSAL.

Related Standards

This material data has been provided by Rusal.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Carbon Footprint

Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al.

Dimension

PropertyValue

Dimensions

9,5 mm

Mechanical

PropertyTemperatureValueComment

Tensile strength

23.0 °C

110 MPa

Show Supplier Material materials with Tensile strength of 110 MPa

min

Electrical

PropertyValueComment

Specific Electrical conductivity

60.5 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 60.5 % IACS

min

Chemical properties

PropertyValue

Aluminium

Balance

Iron

0.25 %

Show Supplier Material materials with Iron of 0.25 %

Silicon

0.08 %

Show Supplier Material materials with Silicon of 0.08 %

Zirconium

0.15 - 0.4 %

Show Supplier Material materials with Zirconium of 0.15 - 0.4 %

Technological properties

Property
Application areas

Thermal resistant electric conductors

Processing history

Smelters: Irkutsk Aluminium Smelter (IrKAZ)