ALLOW™ Slab Series 5182

Want to keep this datasheet? Save it now in your required format

Description

Low Carbon Slabs ALLOW™ produced with renewable hydropower by RUSAL.

Related Standards

Equivalent Materials

This material data has been provided by Rusal.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Carbon Footprint

Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al.

Dimension

PropertyValue

Dimensions

Cross section: 500x2130 mm, 560x1100 mm, 560x1230 mm, 560x1310 mm

Chemical properties

PropertyValueComment

Aluminium

Balance

Chromium

0.1 %

Show Supplier Material materials with Chromium of 0.1 %

according to DIN EN 573-3

Copper

0.15 %

Show Supplier Material materials with Copper of 0.15 %

according to DIN EN 573-3

Iron

0.35 %

Show Supplier Material materials with Iron of 0.35 %

according to DIN EN 573-3

Magnesium

4 - 5 %

Show Supplier Material materials with Magnesium of 4 - 5 %

according to DIN EN 573-3

Manganese

0.2 - 0.5 %

Show Supplier Material materials with Manganese of 0.2 - 0.5 %

according to DIN EN 573-3

Other

0.05 - 0.15 %

Show Supplier Material materials with Other of 0.05 - 0.15 %

according to DIN EN 573-3

Silicon

0.2 %

Show Supplier Material materials with Silicon of 0.2 %

according to DIN EN 573-3

Titanium

0.1 %

Show Supplier Material materials with Titanium of 0.1 %

according to DIN EN 573-3

Zinc

0.25 %

Show Supplier Material materials with Zinc of 0.25 %

according to DIN EN 573-3

Technological properties

Property
Application areas

Aluminium can end

Processing history

Smelters: Bratsk Aluminium Smelter (BrAZ)