Aluminosilicate Glass SCHOTT 8240

Alternative and trade names
SCHOTT 8240
Want to keep this datasheet? Save it now in your required format

Description

For sealing to molybdenum, intensively blue colored alkaline earth aluminosilicate glass, free from alkali, defined absorption. High hydrolytic resistance, high resistance to thermal shock and high temperature resistance.

This material data has been provided by Schott Glass Tubing.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

2.67 g/cm³

Show Supplier Material materials with Density of 2.67 g/cm³

Mechanical

PropertyValue

Elastic modulus

83 GPa

Show Supplier Material materials with Elastic modulus of 83 GPa

Poisson's ratio

0.23 [-]

Show Supplier Material materials with Poisson's ratio of 0.23 [-]

Thermal

PropertyTemperatureValueTesting StandardComment

Annealing temperature

795.0 °C

Show Supplier Material materials with Annealing temperature of 795.0 °C

ISO 7884-4

Viscosity 10¹³ dPa·s

Coefficient of thermal expansion

4.7e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 4.7e-06 1/K

ISO 7991

mean value for 20-300 °C

Glass transition temperature

790 °C

Show Supplier Material materials with Glass transition temperature of 790 °C

ISO 7884-8

Softening temperature

1005.0 °C

Show Supplier Material materials with Softening temperature of 1005.0 °C

ISO 7884-3

Viscosity 10⁷·⁶ dPa·s

Specific electrical resistance temperature

630.0 °C

Show Supplier Material materials with Specific electrical resistance temperature of 630.0 °C

For ρ=10⁸ Ω·cm

Thermal conductivity

90 °C

1.1 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 1.1 W/(m·K)

Working temperature

1305.0 °C

Show Supplier Material materials with Working temperature of 1305.0 °C

ISO 7884-2

Viscosity 10⁴ dPa·s

Electrical

PropertyTemperatureValueFrequency

Dielectric constant

6.6 [-]

Show Supplier Material materials with Dielectric constant of 6.6 [-]

1MHz

Electrical resistivity

250 °C

1e+11 Ω·m

Show Supplier Material materials with Electrical resistivity of 1e+11 Ω·m

350 °C

1e+09 Ω·m

Show Supplier Material materials with Electrical resistivity of 1e+09 Ω·m

Loss tangent

0.0015 [-]

Show Supplier Material materials with Loss tangent of 0.0015 [-]

1MHz

Optical

PropertyValueTesting StandardComment

Refractive index

1.5 [-]

Show Supplier Material materials with Refractive index of 1.5 [-]

at λ=587.6 nm

Stress optical coefficient

2.7e-06 mm²/N

Show Supplier Material materials with Stress optical coefficient of 2.7e-06 mm²/N

DIN 52314

Chemical properties

Property

Other

0.01 %

max., Lead, Cadmium, Mercury and Hexavalent Chromium

Technological properties

Property
Application areas

For high temperature applications in electrical engineering. For use in bulb and exhaust tube for halogen lamps for automotive, houshold and general lighting.

Corrosion properties

Hydrolytic resistance Class HGB1 (ISO 719) - Acid resistance Class S2 (DIN 12116) - Alkali resistance Class A2 (ISO695)