Tribotecc® BIS 84 Bismuth Sulfide is a powder with a high bismuth content (80 %) and purity (at least 98.5%).

The key benefits of Tribotecc® BIS 84 as an additive are:

  • Low melting point
  • High electrical resistance
  • Low Mohs hardness
  • Forms protective layers of different contact surfaces over a wide temperature and pressure range
  • Excellent tribological characteristics
  • Contains bismuth as a non-toxic substitute instead of toxic heavy metals

  • This material data has been provided by Tribotecc.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueComment

    Density

    6.8 g/cm³

    Show Supplier Material materials with Density of 6.8 g/cm³

    Particle size D50

    2 μm

    Show Supplier Material materials with Particle size D50 of 2 μm

    Particle size D90

    5 μm

    Show Supplier Material materials with Particle size D90 of 5 μm

    Sieve residue 45μm

    1.0 %

    Show Supplier Material materials with Sieve residue 45μm of 1.0 %

    max.

    Volatile share

    0.1 %

    Show Supplier Material materials with Volatile share of 0.1 %

    at 105°C

    Mechanical

    PropertyValue

    Hardness, Mohs

    2 [-]

    Show Supplier Material materials with Hardness, Mohs of 2 [-]

    Thermal

    PropertyValueComment

    Max service temperature

    400.0 °C

    Show Supplier Material materials with Max service temperature of 400.0 °C

    Melting point

    685.0 °C

    Show Supplier Material materials with Melting point of 685.0 °C

    Oxidation threshold

    400.0 °C

    Show Supplier Material materials with Oxidation threshold of 400.0 °C

    min.

    Specific heat capacity

    280.0 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 280.0 J/(kg·K)

    Thermal conductivity

    0.379 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.379 W/(m·K)

    Thermal diffusivity

    0.252 mm²/s

    Show Supplier Material materials with Thermal diffusivity of 0.252 mm²/s

    Electrical

    PropertyValue

    Electrical conductivity

    0.061 S/m

    Show Supplier Material materials with Electrical conductivity of 0.061 S/m

    Electrical resistivity

    16.0 Ω·m

    Show Supplier Material materials with Electrical resistivity of 16.0 Ω·m

    Chemical properties

    PropertyValue

    Bismuth

    80.0 %

    Show Supplier Material materials with Bismuth of 80.0 %

    Sulfur

    17.0 - 20.0 %

    Show Supplier Material materials with Sulfur of 17.0 - 20.0 %

    Technological properties

    Property
    Application areas

    Tribotecc® BIS 84 bismuth sulfide is characterised by a particularly low melting point and low metal hardness.

    Combined with the ability to form protective layers of different contact surfaces over a wide range of temperatures and pressures, and excellent wear, friction and alloying properties as an additive, this product is ideal for a wide range of applications:

    E.g. in the plastics-, automotive-, machinery- and construction industries as well as in ceramics and medical technology.

    Color

    Grey