Tribotecc® MOS XF Molybdenum Disulfide

Want to keep this datasheet? Save it now in your required format

Description

The key benefits of Tribotecc® MOS XF are: Carefully selected raw material, polar chemical bond, low hardness, layer lattice structure

This material data has been provided by Tribotecc.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

4.8 g/cm³

Show Supplier Material materials with Density of 4.8 g/cm³

Particle size D50

10 μm

Show Supplier Material materials with Particle size D50 of 10 μm

Particle size D90

23 μm

Show Supplier Material materials with Particle size D90 of 23 μm

Chemical properties

PropertyValue

Molybdenum

57.0 %

Show Supplier Material materials with Molybdenum of 57.0 %

Technological properties

Property
Application areas

Friction: Disc brake pads, clutch facings, brake linings to improve pad and disc wear and NVH-characteristics; Lubricants: Greases, pastes and oils to reduce coefficient of friction and wear and improve emergency running properties; Plastics: Highly engineered thermoplastics to improve wear and durability; Powder metallurgy: Reduces wear in sintered parts; Other applications: Diamond/CBN tools, coatings, powder metallurgy, metal forming, carbon brushes

Color

Dark grey