Tribotecc® SLS 22 Tin sulfides, Phosphates

Want to keep this datasheet? Save it now in your required format

Description

Tribotecc® SLS 22 is a synergistic compound of selected high purity inorganic materials based on tin disulfides and phosphates. It can be used as a solid lubricant and many other fields of application. The key benefits of Tribotecc® SLS 22 are:

  • A significant reduction of coefficient of friction and wear
  • An improvement of emergency running properties
  • An improvement of sliding, rotating friction and durability
  • The formation of stable layers of different contact surfaces over a wide temperature and pressure range
  • Excellent tribological characteristics

  • This material data has been provided by Tribotecc.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueComment

    Density

    3.1 g/cm³

    Show Supplier Material materials with Density of 3.1 g/cm³

    Particle size D50

    8 μm

    Show Supplier Material materials with Particle size D50 of 8 μm

    Particle size D90

    24 μm

    Show Supplier Material materials with Particle size D90 of 24 μm

    Poured density

    0.75 g/cm²

    Show Supplier Material materials with Poured density of 0.75 g/cm²

    1 g/cm²

    Show Supplier Material materials with Poured density of 1 g/cm²

    Sieve residue 45μm

    4.0 %

    Show Supplier Material materials with Sieve residue 45μm of 4.0 %

    max.

    Tamped Volume

    60 ml/100g

    Show Supplier Material materials with Tamped Volume of 60 ml/100g

    90 ml/100g

    Show Supplier Material materials with Tamped Volume of 90 ml/100g

    Volatile share

    0.1 %

    Show Supplier Material materials with Volatile share of 0.1 %

    at 105°C

    Thermal

    PropertyValueComment

    Max service temperature

    400.0 °C

    Show Supplier Material materials with Max service temperature of 400.0 °C

    Oxidation threshold

    400.0 °C

    Show Supplier Material materials with Oxidation threshold of 400.0 °C

    min.

    Chemical properties

    PropertyValue

    Calcium

    29.0 %

    Show Supplier Material materials with Calcium of 29.0 %

    Tin

    4.5 %

    Show Supplier Material materials with Tin of 4.5 %

    Technological properties

    Property
    Application areas

    Tribotecc® SLS 22 is characterized by its excellent tribological characteristics. Combined with the ability to form stable layers of different contact surfaces over a wide range of temperatures and pressures, and excellent wear and friction properties, this product is ideal for a wide range of

    applications: E.g. as an additive in lubricants in the form of greases, pastes and oils; in the plastic industry; powder metallurgy; as coatings in general;

    Color

    Bright