Tribotecc® SNS 2 Grade A Tin Sulfide and Tin Disulfide (98.5% purity)

Want to keep this datasheet? Save it now in your required format

Description

The key benefits of SNS 2 Grade A are: Fully synthetic unique solid lubricant, high load capacity, reduce coefficient of friction and wear under extreme pressures.

This material data has been provided by Tribotecc.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

4.5 g/cm³

Show Supplier Material materials with Density of 4.5 g/cm³

Particle size D50

3 μm

Show Supplier Material materials with Particle size D50 of 3 μm

Particle size D90

9 μm

Show Supplier Material materials with Particle size D90 of 9 μm

Thermal

PropertyValue

Max service temperature

400.0 °C

Show Supplier Material materials with Max service temperature of 400.0 °C

Chemical properties

PropertyValue

Tin

64.0 %

Show Supplier Material materials with Tin of 64.0 %

Technological properties

Property
Application areas

Friction: High tech friction materials to improve pad and disc wear; NVH characteristics; Lubricants: Greases, pastes and oils to reduce coefficient of friction and wear and improve emergency running properties; Plastics: Highly engineered thermoplastics to improve wear and durability; Other applications: Coatings, powder metallurgy, carbon brushes

Color

Mosaic-gold