Tribotecc® CB 500 Copper-(II)-sulfide is a blue black and fully synthetic powder with a purity (>99 %). The key benefits of Tribotecc® CB 500 as an additive are:

  • Excellent absorbens and catalytical properties
  • Active material for batteries
  • High melting point
  • Increases corrosion-resistance
  • Stable layers of different contact surfaces over a wide temperature and pressure range
  • Excellent tribological characteristics und extensibility

  • This material data has been provided by Tribotecc.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    4.3 - 4.9 g/cm³

    Show Supplier Material materials with Density of 4.3 - 4.9 g/cm³

    Particle size D50

    7 - 30 μm

    Show Supplier Material materials with Particle size D50 of 7 - 30 μm

    Particle size D90

    15 - 40 μm

    Show Supplier Material materials with Particle size D90 of 15 - 40 μm

    Volatile share

    0.5 %

    Show Supplier Material materials with Volatile share of 0.5 %

    at 105°C

    Thermal

    PropertyTemperatureValueComment

    Max service temperature

    400 °C

    Show Supplier Material materials with Max service temperature of 400 °C

    Melting point

    1100 °C

    Show Supplier Material materials with Melting point of 1100 °C

    Oxidation threshold

    400 °C

    Show Supplier Material materials with Oxidation threshold of 400 °C

    min.

    Specific heat capacity

    23.0 °C

    324 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 324 J/(kg·K)

    Thermal conductivity

    23.0 °C

    1.13 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 1.13 W/(m·K)

    Thermal diffusivity

    23.0 °C

    1.34 mm²/s

    Show Supplier Material materials with Thermal diffusivity of 1.34 mm²/s

    Electrical

    PropertyTemperatureValue

    Electrical conductivity

    23.0 °C

    140000 S/m

    Show Supplier Material materials with Electrical conductivity of 140000 S/m

    Electrical resistivity

    23.0 °C

    7E-6 Ω·m

    Show Supplier Material materials with Electrical resistivity of 7E-6 Ω·m

    Technological properties

    Property
    Application areas

    Tribotecc® CB 500 Copper-(II)-sulfide is characterised by its excellent absorbens and catalytical properties.

    Combined with the ability to form stable layers of different contact surfaces over a wide range of temperatures and pressures and excellent wear and friction properties as an additive, this product is ideal for a wide range of applications:

    E.g. in the areas of:

  • Catalysts
  • Sorbens
  • Electronic Applications
  • Energy storage
  • Friction
  • Lubricants
  • Plastics industry
  • Automotive industry
  • Machinery industry
  • Construction industry
  • Ceramics

  • Color