General
Property | Value | Related Standards | Shape |
---|---|---|---|
Density | 2.7 g/cm³ Show Material materials with Density of 2.7 g/cm³ | EN 573-3 | Strip, Sheet, Plate |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 69.5 - 70.0 GPa Show Material materials with Elastic modulus of 69.5 - 70.0 GPa | Typical for Wrought 3000 Series Aluminium |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 3000 Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Wrought 3000 Series Aluminium |
Shear modulus | 25.0 - 26.0 GPa Show Material materials with Shear modulus of 25.0 - 26.0 GPa | Typical for Wrought 3000 Series Aluminium |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.2e-05 - 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.4e-05 1/K | Typical for Wrought 3000 Series Aluminium |
Melting point | 629.0 - 654.0 °C Show Material materials with Melting point of 629.0 - 654.0 °C | Typical for Wrought 3000 Series Aluminium |
Specific heat capacity | 893.0 - 920.0 J/(kg·K) Show Material materials with Specific heat capacity of 893.0 - 920.0 J/(kg·K) | Typical for Wrought 3000 Series Aluminium |
Thermal conductivity | 154.0 - 193.0 W/(m·K) Show Material materials with Thermal conductivity of 154.0 - 193.0 W/(m·K) | Typical for Wrought 3000 Series Aluminium |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 23000000.0 - 29000000.0 S/m Show Material materials with Electrical conductivity of 23000000.0 - 29000000.0 S/m | Typical for Wrought 3000 Series Aluminium |
Electrical resistivity | 3.4e-08 - 4.2e-08 Ω·m Show Material materials with Electrical resistivity of 3.4e-08 - 4.2e-08 Ω·m | Typical for Wrought 3000 Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Copper | 0.15 % Show Material materials with Copper of 0.15 % | EN 573-3 | Strip, Sheet, Plate |
Iron | 0.1 % Show Material materials with Iron of 0.1 % | EN 573-3 | |
0.10 % Show Material materials with Iron of 0.10 % | EN 573-3 | Strip, Sheet, Plate | |
Magnesium | 0.05 - 0.2 % Show Material materials with Magnesium of 0.05 - 0.2 % | EN 573-3 | Strip, Sheet, Plate |
Manganese | 0.05 - 0.25 % Show Material materials with Manganese of 0.05 - 0.25 % | EN 573-3 | Strip, Sheet, Plate |
Silicon | 0.08 % Show Material materials with Silicon of 0.08 % | EN 573-3 | Strip, Sheet, Plate |
Titanium | 0.03 % Show Material materials with Titanium of 0.03 % | EN 573-3 | Strip, Sheet, Plate |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % | EN 573-3 | Strip, Sheet, Plate |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % | EN 573-3 | Strip, Sheet, Plate |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |