Alpha-Beta-Legierung
DIN 17851 Grade 3.7185Alpha-Beta-Legierung
DIN 17851 Grade 3.7185Zinc Aluminium
EN 12844 Grade G-ZnAl4Cu3 cast conditionZinc Aluminium
EN 12844 Grade GD-ZnAl4 cast conditionZinc Aluminium
EN 12844 Grade GD-ZnAl4Cu1 cast conditionZinc Aluminium
EN 12844 Grade ZP3Zinc Aluminium
EN 12844 Grade ZP5Zinc Aluminium
EN 12844 Grade ZP2Nickel-Kupfer-Legierung
DIN 17743 Grade NiCu30Al artificially agedFerritischer Edelstahl
DIN 59470 Grade CrAl14-4 soft annealed (+A)Alphalegierung
GOST 22178 Grade OT4Alphalegierung
GOST 22178 Grade OT4Betalegierung
ASTM Grade 19 Solution TreatedBetalegierung
ASTM Grade 19 Moderate StrengthBetalegierung
ASTM Grade 19 High StrengthNickel Chromium Alloy
DIN 17742 Grade NiCr20AlSi soft annealed (+A)Cast Aluminium Manganese Grade
ASTM AS41ACast Aluminium Manganese Grade
ASTM AS41B