Molybdän: 1 - 1.4 %

Quick Comparison

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 12CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 12CrMoV12-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type E Class 4 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type A Class 2 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type D Class 1 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type A Class 1 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Chromium Molybdenum Steel

ASTM A542 Type B Class 1 Quenched and Tempered

Geliefert von:

1 Matmatch-Lieferant

Nickel-Eisen-Legierung

VDM® Alloy 33

Geliefert von:

VDM Metals

Austenitischer rostfreier Stahl

Esshete 1250

Geliefert von:

Alleima (formerly Sandvik Materials Technology)

Duplex rostfreier Stahl

UGIMA® 4460 Cold Finished

Geliefert von:

Ugitech

Duplex rostfreier Stahl

UGIMA® 4460 Cold Finished and Drawn

Geliefert von:

Ugitech

Martensitischer Edelstahl

Acidur 4418 QT900

Geliefert von:

Deutsche Edelstahlwerke (DEW)

Martensitischer Edelstahl

Acidur 4418 QT760

Geliefert von:

Deutsche Edelstahlwerke (DEW)

Martensitischer Edelstahl

UGI 4418 QT900 Turned Bar

Geliefert von:

Ugitech
Seite 1 von 24