Polyamide 6T (PA6T)
Zytel® HTN51G35HSL NC010Polyamide 66 (PA66)
Minlon® 11C140 NC010Polybutylenterephthalat (PBT)
Crastin® SK602 NC010Polybutylenterephthalat (PBT)
Crastin® SK603 NC010Polyamide 66 (PA66)
Zytel® 70G50HSLA BK039BPolybutylenterephthalat (PBT)
Crastin® HR5330HF NC010Polybutylenterephthalat (PBT)
Crastin® SK605 NC010Polyamide 66 (PA66)
Zytel® FR70M30V0 NC010Polymermischung (Blend)
Crastin® LW9020 NC010Polyethylenterephthalat (PET)
Rynite® 935 NC010Polymermischung (Blend)
Crastin® LW9030 NC010Polybutylenterephthalat (PBT)
Crastin® SK601 NC010Polybutylenterephthalat (PBT)
Crastin® HR5315HF NC010Polymermischung (Blend)
Crastin® LW9030FR NC010Polyethylenterephthalat (PET)
Rynite® FR530 NC010Polyamide 66 (PA66)
Minlon® EFE6053 BK413Polybutylenterephthalat (PBT)
Crastin® SO653 NC010Polyamide 66 (PA66)
Zytel® FG70G50HSLA BK309Polybutylenterephthalat (PBT)
Crastin® T843FR NC010