Kohlenstoffarmer Stahl
EN 10025-2 Grade S355J2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10025-2 Grade S355K2 normalized or normalized formed (+N)Geliefert von:
2 Matmatch-Lieferanten
Kohlenstoffarmer Stahl
EN 10209 Grade DC01EK cold rolled, skin passedGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10209 Grade DC04EK cold rolled, skin passedGeliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10149-3 Grade S315NC normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
EN 10207 Grade P235S normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Kohlenstoffarmer Stahl
DIN 17103 Grade TStE 285 normalized or normalized formed (+N)