Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Molybdenum Steel
EN 10028-2 Grade 16Mo3 normalized or normalized formed (+N)Suministrada por:
2 proveedores de Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 10CrMo9-10 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Acero inoxidable austenítico
Esshete 1250Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
Sanicro® 25Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable dúplex
Sandvik SAF 2707 HD™Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiMoN17-13-5 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiN18-10 solution annealed (+AT)