Mezcla de polímeros
Crastin® LW9020 NC010Polioximetileno (POM)
Delrin® 900P NC010Tereftalato de polibutileno (PBT)
RADITER B RV200 100 NTSuministrada por:
RadiciGroup High Performance PolymersPolyamide 66 (PA66)
Minlon® EFE6096 GY090ACopolyamide 6I/6T (PA6I/6T)
RADILON AESTUS T1 RV300FC 306K BKSuministrada por:
RadiciGroup High Performance PolymersPolyamide 66 (PA66)
Zytel® BM70G20HSLX BK537Polioximetileno (POM)
Delrin® 100AL NC010Polioximetileno (POM)
Delrin® SC699 NC010Polipropileno
Polypropylene Reinforced with 30% Glass Fibre (PP+GF30)Suministrada por:
1 proveedor Matmatch
Tereftalato de polibutileno (PBT)
Polybutylene terephthalate Reinforced with 30% Glass Fibre (PBT+GF30)Suministrada por:
4 proveedores de Matmatch
Poliftalamida (PPA)
Polyphthalamide Reinforced with 33% Glass Fibre (PPA+GF33)Suministrada por:
2 proveedores de Matmatch
Poliéter éter cetona (PEEK)
Polyetheretherketone Reinforced with 30% Glass Fibre (PEEK+GF30)Suministrada por:
1 proveedor Matmatch
Poliéter éter cetona (PEEK)
Polyetheretherketone Reinforced with 30% Carbon Fibre (PEEK+CF30)Suministrada por:
2 proveedores de Matmatch
Polipropileno
Polypropylene Reinforced with 40% Mineral (PP+M40)Suministrada por:
2 proveedores de Matmatch